    Jeez...meet, I can't spell or type or both.
  • image
    image
    Laguna skimping on my alumina...next thing you know they'll be sneaking 10 percent tofu into the mix like Taco Bell does with their meet just to save themselves a little EPK.
  • Covered jar
    Covered jar
    Marko, anytime. You are in the area you are welcome, best to give as much notice as possible in case I'm out running around in the mountains so I can be sure and be around to see you.
  • Covered jar
    Covered jar
    Really good pottery in modesty. If I ever get to Santa Clara, for sure I would stop by your studio.
  • image
    image
    Go cheap on the amount of alumina in a clay body: does the same thing.