    Pieter:When I have chemically etched materials they separate out into carbons, solids, and metals. I would agree soluble salts are clinging to the sides: but by chance are those carbons floating? I...
  • IMG 0002
    IMG 0002
    This is just calcined Colemanite in some water in a polystyrene cup. See my post in this thread for more context:http://community.ceramicartsdaily.org/topic/15955-colemanite/ I think the light...
  • TLH SYOM 33 NO4
    TLH SYOM 33 NO4
    I just added a pic with the stamp, which I had forgotten to do. The color of the piece is accurate in this view-looks too pinklish in the other pic.
  • Micro crystals
    Micro crystals
    Mark:I agree. What amazes me even more is that when you zoom in, all the color disappears. No matter what color the glaze is, under high magnification most, if not all goes away. Says something abo...
  • Celadon
    Celadon
    Very nice. Can you add some close-ups, please? Nice form and fluting.




Recent Images



  • 1,085 Total Albums
  • 8,053 Total Images
  • 3,149 Total Comments
  • 1.35GB Total Gallery Size