Blending various blends of raw clay to set levels of titanium, iron, and calcium. The goal was to produce purple in oxidation: without the use of stains. A band of rutile was placed in the center, and Temmoku glazed over.


Copyright

© TJA 2017
Sign in to follow this  

Photo Information for Titanium, calcium, iron clay body


Recommended Comments

There are no comments to display.

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.