last of the leaves and the shape of the mold allows me to add another dragonfly in the empty section. flexibility is what i want with this mold. i can make small squares using the first end and butterdishes and trays using the rest of it. now to dry it totally flat between drywall sheets. they are turned about twice a day until totally dry. this will be fired to 04 and used to give texture to slabs that will be made into trays, etc. rolling the slabs to pick up the leaf texture is done with a foam backing under the mold to absorb the pressure.