For those exploring crystalline glazes: these tiles show how zinc is used to control crystal growth.

Tile 1: 25% Tile 2: 26% Tile 3: 27% (left side)

Copyright

© TJA 2017

From the album:

crystals

· 17 images
  • 17 images
  • 0 comments
  • 13 image comments

Photo Information

  • Taken with EASTMAN KODAK COMPANY KODAK EASYSHARE C182 Digital Camera
  • Focal Length 7.1 mm
  • Exposure Time 12500/1000000
  • f Aperture f/3.2
  • ISO Speed 160

Recommended Comments

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.