glazenerd 1,807 Posted September 24, 2016 Report Share Got a very close up of the wall cavity by chance? Quote Link to comment
1515art 260 Posted September 24, 2016 Report Share The iPhone 5 has its limitations, I broke about a third of the cups in half after testing the ring sound with a small metal hammer. The ones with a dull sound I broke in half and most show shiny black carbon deposits. also had very uneven firing, the way I loaded the kiln may have been some of the problem and my burners may need a little work. Quote Link to comment