I set a challenge for myself at the beggining of the year to throw more bottles.

Here is one such piece. Straight up ferric chloride coating.


Sign in to follow this  
From the album:

Ferric Chloride

  • 13 images
  • 0 comments
  • 20 image comments

Photo Information for 04171617

Taken with Canon Canon EOS DIGITAL REBEL XTi

  • 48 mm
  • 1/500
  • f f/14.0
  • ISO 400
View all photo EXIF information

Recommended Comments

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.