Butterfly mug

firenflux
Sign in to follow this  

This was a new take on a design I've been doing awhile. It may have spurred a new variation on several of my usual pots. I'm excited to see what comes of it.

 

The pattern at the bottom was created with paper resist and sgraffito. After bisque fired, black underglaze was applied and wiped back, then colorful accents added to the wings. It's finished with commercial ial glazes and fired to cone 6 in an electric kiln.


Sign in to follow this  
From the album:

Favorites

  • 21 images
  • 0 comments
  • 20 image comments

Photo Information for Butterfly mug


Recommended Comments

There are no comments to display.

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.