After reading CAD article about making your own transfers, I tried this using a rubber stamp with stain & frit 50:50 mix. Stamped on to tissue paper, applied to leather hard clay. Bisqued to 1000oC. Dipped in transparent glaze & fired to 1100oC in an electric kiln.


Sign in to follow this  
From the album:

2016

  • 6 images
  • 0 comments
  • 5 image comments


Recommended Comments

There are no comments to display.

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.