platter with peaches some color applied
slip and underglaze to give color to the fruit and rim, washed with red iron oxide. peaches covered with weighted craft foam cut to fit fruit shapes. glaze sprayed over all. fired to cone 6. some colors washed out or were too thinly applied so a second firing was necessary to complete the piece.