I slipped this container into a tall spot in the kiln at the last minute to see how my glazes break over the undulating walls. Actually, I really needed the pot for the Anthurium that I received as a birthday gift back in January...it was quite root bound and begging for better living conditions.

 

Container is about 13" tall, stoneware, fired to cone 10 reduction and glazed with a combination of Ohio White, Woo's Blue, and Clear (sprayed on in overlapping layers).


Copyright

© Copyright 2015, Paul M. Chenoweth, Nashville, TN. All rights reserved.
Sign in to follow this  
From the album:

Tornado Pot Sketches and Progress Images

  • 15 images
  • 0 comments
  • 40 image comments

Photo Information for Anthurium Couldn't Wait


Recommended Comments

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.