Jump to content

Gas bubbles


Crusty

I used a white,red and Black Raven slip with a clear gloss on this. The red and white did fine , the black released more gasses.. it was bisque fired to ^04 and was actually a little over fired according to the small cone..

From the album:

Black Raven

· 1 image
  • 1 image
  • 0 comments
  • 0 image comments

Photo Information

  • Taken with Canon Canon EOS DIGITAL REBEL XTi
  • Focal Length 56 mm
  • Exposure Time 1/320
  • f Aperture f/11.0
  • ISO Speed 1600

Recommended Comments

There are no comments to display.

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.