Wood And Gas Teapots
Two teapots I threw at a workshop by Kevin Crowe. The one on the left was wood fired at the Michael Kline "Stoketember" workshop at Arrowmont. It only had a slip called bisque flash on it. The one on the right was gas fired with a shino glaze and some wood ash thrown on the shoulders. Both are Phoenix 10 clay.