The latest Luminary lamp that I used different colors to see the effect had cracked in the drying stage and when the inside light was turned on, gave this wonderful orange glow from the skyscraper to the alien ship. I couldn't produce that again if I tried.

Sign in to follow this  
From the album:

flasks

  • 32 images
  • 0 comments
  • 6 image comments

Photo Information for large colored Luminary lamp (that cracked in the perfect spot)

Taken with Apple iPhone 4S

  • 4.3 mm
  • 1/28
  • f f/2.4
  • ISO 64
View all photo EXIF information

Recommended Comments

There are no comments to display.

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.