My first raku

From the album:

Raku

· 9 images
  • 9 images
  • 0 comments
  • 4 image comments

Photo Information


Recommended Comments

pictures don't show it but in some pieces there is an iridescent/metallic quality in areas,  i had others use it and didn't get same effect.   i pulled from kiln onto news paper, placed more newspaper, closed lid on trash/redux can...... repeat