Other images in Enamel - microscope photos of surface

finelymixed

This is a result of finely mixing ( with some grinding) standard enamel powders (intended for copper) shown at a magnification of 400x. The enamels were fired for a few minutes by torch at an estimated temperature of 850 C / 1562 F

 

It shows almost no color blending - I was hoping for a little "fuzziness" at least.