Youhen Flower Arranging Vase
 
© John Baymore 2013 - all rights reserved
Image Tools

Youhen Flower Arranging Vase

Guest
Sign in to follow this  
  • 844 views

Thrown; yakishime; youhen charcoal finish; noborigama woodfired at Kanayamayaki, Goshogawara-shi, Aomori-ken, Japan; Orton cone 14. Private collection in Japan.


Copyright

© John Baymore 2013 - all rights reserved
Sign in to follow this  
From the album:

John Baymore's Clay Work

  • 31 images
  • 0 comments
  • 38 image comments

Photo Information for Youhen Flower Arranging Vase

Taken with Canon Canon PowerShot SX160 IS

  • 15.9 mm
  • 1/4
  • f f/8.0
  • ISO 100
View all photo EXIF information

Recommended Comments

There are no comments to display.

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
×

Important Information

By using this site, you agree to our Terms of Use.