From the Inside, Out
Thrown, assembled, and altered "Red Art" earthenware, colored slips and underglazes, fired to 04. Ink wash and oil paint. Fabricated Nickel Silver stand.
2.5" x 4.5" x 5"
Thrown, assembled, and altered "Red Art" earthenware, colored slips and underglazes, fired to 04. Ink wash and oil paint. Fabricated Nickel Silver stand.
2.5" x 4.5" x 5"