Recommended Comments

Hey JohnnyK, Around the rim, where the glaze is lighter, is Strontium Crystal Magic Cool sprayed on. Then Pete's Seafoam is sprayed over the whole piece. The SCMC makes Pete's Seafoam go turquoise. Depending on thickness of Pete's Seafoam, on non-SCMC areas, will result in the varied amount of splotches. The army green color is where Pete's Seafoam is thinner. 

Thank you

Share this comment


Link to comment

My first time on here this morning and what a beautiful glaze! 

Not sure what Pete’s Sea Foam is but it is a lovely colour

Share this comment


Link to comment

Thank you all for your kind words. Joseph, as you know, it takes time to sort out the glazes and how to apply each one.

Pete's Seafoam is a glaze recipe created by Pete Pinnell.

Share this comment


Link to comment

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.